Material | Attributes | Tensile Strength | Yield Strength | Elongation | ||||
---|---|---|---|---|---|---|---|---|
As Printed |
With Heat Treatment | As Printed | With Heat Treatment | As Printed | With Heat Treatment | |||
Aluminum AlSi10Mg |
Corrosion resistance, high strength-to-weight ratio and temperature resistance | 70 ksi | 42 ksi | 42 ksi | 26 ksi | 3-6% | 11%+ | |
Aluminum F357 |
Corrosion resistance, high strength-to-weight ratio and temperature resistance | 61 ksi | 47 ksi | 42 ksi | 40 ksi | 3-6% | 11.5%+ | |
Aluminum A6061-RAM2 |
Great strength to weight ratio. Excellent corrosion and machinability | 45 ksi | 45 ksi | 40 ksi | 41 ksi | 14% | 11% | |
Copper GRCop-42 |
Combination of high heat flux, high conduction and high strength. Good material strength at high temperatures . Oxidation and blanching resistnace. | 78 ksi | 53 ksi | 48 ksi | 28 ksi | 23% | 31%+ | |
Cobalt Chrome CoCrMo |
High tensile strength & hardness; bio-compatibility | 153 ksi | 135 ksi | 121 ksi | 82 ksi | 8-10% | 20% | |
Hastelloy X | High strength and oxidation and crack resistance | 112 ksi | 125 ksi | 87.5 ksi | 105 ksi | 18-20% | 34% | |
Inconel 718 |
High strength, excellent temperature and corrosion resistance | 140 ksi | 196 ksi | 88 ksi | 166 ksi | 30% | 17% | |
Inconel 625 |
Excellent fatigue properties along with increased oxidation resistance | 70 ksi | 168 ksi | 40 ksi | 67 ksi | 30% | 15% | |
Inconel H282 |
High strength in high temperature situations, including high creep. Gamma prime strengthened and easily fabricated. | 138 ksi | 130 ksi | 40 ksi | 97 ksi | 47% | 53% | |
Niobium C103 | Excellent mechanical properties at extreme temperatures | 93 ksi | 73 ksi | 76 ksi | 53 ksi | 30% | 32% | |
Stainless Steel 17-4 |
High strength and hardness with good corrosion resistance | 120 ksi | 160 ksi | 83 ksi | 150 ksi | 15% | 20% | |
Stainless Steel 316L |
Corrosion and crack resistance | 97 ksi | 80 ksi | 72 ksi | 40 ksi | 50% | 60% | |
Titanium TiAl6V4 |
Corrosion resistance, strength, temperature resistance and weight reduction | 186 ksi | 155 ksi | 161 ksi | 141 ksi | 12% | 18% |
Properties referenced are approximate. Parameters, processes, orientation, and location on build plate can impact final build outcomes. This table is for reference only.