GO BACK TO HOME
Materials Guide
Material Attributes Tensile Strength Yield Strength Elongation
As Printed With Heat Treatment & HIP As Printed With Heat Treatment or HIP As Printed With Heat Treatment & HIP
Aluminum
AlSi10Mg
Corrosion resistance, high strength-to-weight ratio and temperature resistance 70 ksi 42 ksi 42 ksi 26 ksi 3-6% 11%+
Aluminum
F357
Corrosion resistance, high strength-to-weight ratio and temperature resistance 61 ksi 40 ksi 42 ksi 24 ksi 3-6% 11%+
Cobalt Chrome
CoCrMo
High tensile strength & hardness; bio-compatibility 153 ksi 135 ksi 121 ksi 82 ksi 8-10% 20%
Hastelloy X High strength and oxidation and crack resistance 112 ksi 125 ksi 87.5 ksi 105 ksi 18-20% 34%
Inconel
718
High strength, excellent temperature and corrosion resistance 140 ksi 196 ksi 88 ksi 166 ksi 30% 17%
Inconel
625
Excellent fatigue properties along with increased oxidation resistance 70 ksi 130 ksi 40 ksi 67 ksi 30% 15%
Stainless Steel
17-4
High strength and hardness with good corrosion resistance 120 ksi 160 ksi 83 ksi 150 ksi 15% 20%
Stainless Steel
316L
Corrosion and crack resistance 97 ksi 80 ksi 72 ksi 40 ksi 50% 60%
Titanium
TiAl6V4
Corrosion resistance, strength, temperature resistance and weight reduction 186 ksi 155 ksi 161 ksi 141 ksi 12% 18%

Properties referenced are approximate. Parameters, processes, orientation, and location on build plate can impact final build outcomes. This table is for reference only.

Sintavia’s powder laboratory is ISO 17025/ANAB accredited. 